In a UTM experiment a sample of length 100 mm, was loaded in tension until failure. The failure load was 40 kN. The displacement

Q. In a UTM experiment, a sample of length 100 mm, was loaded in tension until failure. The failure load was 40 kN. The displacement, measured using the cross-head motion, at failure, was 15 mm. The compliance of the UTM is constant and is given by 5 × 10−8 m/N. The strain at failure in the sample is____%.

Ans: 12-14